MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance toughness of the structure. This product is a low gel MAH-grafted elastomer useful to improve impact resistance for polyamide or other engineering resins and to enhance interlayer adhesion in co-extruded films.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.8985 g/cc0.03246 lb/in³ASTM D792
Filler Content 0.25 - 0.50 %0.25 - 0.50 %MAH graft; Dow Method
Melt Flow 3.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90905 sec; ASTM D2240
 91911 sec; ASTM D2240
Tensile Strength, Ultimate 11.0 MPa1600 psiASTM D638
Elongation at Break 900 %900 %ASTM D638
Flexural Modulus 0.103 GPa
@Strain 2 %
15.0 ksi
@Strain 2 %
Secant; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 117 °C243 °FDow Method
Glass Transition Temp, Tg -47.0 °C-52.6 °FDow Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AMPLIFY™ GR 202 Maleic anhydride grafted (MAH) polymer
Dow AMPLIFY™ GR 207 Maleic anhydride grafted (MAH) polymer
Dow AMPLIFY™ GR 205 Maleic anhydride grafted (MAH) polymer
Dow AMPLIFY™ GR 209 Maleic anhydride grafted (MAH) polymer
Eastman Saflex® Hurricane Interlayer

PDOW1187 / 30405

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.