MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.

It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. It is used in the automotive industry and electrical sectors.

This product is available in colors on request.

Glow wire test thick. 1,6 mm, IEC 695-2-1, is 650°C. Glow wire test thick. 1,6 mm:<5s, IEC 695-2-1/HN60-E-02, is 650°C.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 6; PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ISO 1183-A
Water Absorption 0.95 %0.95 %24 hours in water at 23°C; ISO 62.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 190 MPa27600 psiISO 527
Elongation at Break 3.8 %3.8 %ISO 527
Tensile Modulus 9.60 GPa1390 ksiISO 527
Flexural Yield Strength 280 MPa40600 psiISO 178
Flexural Modulus 9.50 GPa1380 ksiISO 178
Izod Impact Resistance 1.40 J/cm²6.66 ft-lb/in²ISO 180
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179/1EA-1993
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1EA-1993
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 93
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 V550 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
17.8 µin/in-°F
@Temperature 73.4 - 185 °F
ASTM E831
Melting Point 222 °C432 °FISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
ISO 1210/UL 94
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
ISO 1210/UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 225 - 230 °C437 - 446 °F
Middle Barrel Temperature 230 - 240 °C446 - 464 °F
Front Barrel Temperature 240 - 250 °C464 - 482 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry

PRHO14 / 65948

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.