MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Seals Eastern 5725 Fluorocarbon-Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Formulated Viton®. General service.

Information provided by Seals Eastern, Inc.

Key Words: FKM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.03 g/cc2.03 g/ccASTM D297, 15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 85>= 85ASTM D2240, Type A
 9595AVG; ASTM D2240, Type A
Tensile Strength at Break >= 8.170 MPa>= 1185 psiASTM D412 Method A
 11.98 MPa1737 psiAVG; ASTM D412 Method A
Tensile Stress at Strain  >= 4.46 MPa
@Strain 50 %
>= 647 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 4.86 MPa
@Strain 25 %
705 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 5.53 MPa
@Strain 100 %
>= 802 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 5.83 MPa
@Strain 50 %
845 psi
@Strain 50 %
Average; ASTM D412 Method A
 8.046 MPa
@Strain 100 %
1167 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 84 %>= 84 %ASTM D412 Method A
 200 %200 %AVG; ASTM D412 Method A
Modulus of Elasticity 0.04430 GPa6.425 ksiASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.01477 GPa2.142 ksiASTM D412 Method A
Secant Modulus 0.0416 GPa6.04 ksiASTM D412 Method A
Tear Strength Test 300300(psi); ASTM D624, Die B
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -20.0 °C-4.00 °FASTM D1329
 
Processing PropertiesMetricEnglishComments
Shelf Life 240 Month240 MonthASTM D395, Test B
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)98

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 5724 Fluorocarbon-Elastomer
Cri-Tech FDA-615 FKM Fluoroelastomer, Durometer 61A
Seals Eastern 5722 Fluorocarbon-Elastomer
Process Technologies Inc FKM/Metal - Metal Detectable Sanitary Gasket
Cri-Tech FDA-615-65-THK FKM Fluoroelastomer, Durometer 66A

PSEAL34 / 80181

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.