MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low Temperature

Application: IT/OA Housing and Components

CAS: 103598-77-2 and 143106-82-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
12 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 117117ASTM D785
Tensile Strength, Yield 54.9 MPa
@Thickness 3.20 mm
7970 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 100 %
@Thickness 3.20 mm
100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 88.3 MPa
@Thickness 3.20 mm
12800 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.16 GPa
@Thickness 3.20 mm
313 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched  >= 2.94 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
>= 5.51 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 >= 5.88 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
>= 11.0 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 125 °C
@Thickness 6.40 mm
>= 257 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  80.0 °C
@Thickness >=1.60 mm
176 °F
@Thickness >=0.0630 in
 80.0 °C
@Thickness >=3.20 mm
176 °F
@Thickness >=0.126 in
UL RTI, Mechanical with Impact  80.0 °C
@Thickness >=1.60 mm
176 °F
@Thickness >=0.0630 in
 80.0 °C
@Thickness >=3.20 mm
176 °F
@Thickness >=0.126 in
UL RTI, Mechanical without Impact  80.0 °C
@Thickness >=1.60 mm
176 °F
@Thickness >=0.0630 in
 80.0 °C
@Thickness >=3.20 mm
176 °F
@Thickness >=0.126 in
Flammability, UL94  V-0
@Thickness >=1.60 mm
V-0
@Thickness >=0.0630 in
 V-0
@Thickness >=3.20 mm
V-0
@Thickness >=0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 275 - 290 °C527 - 554 °FInjection Molding
Middle Barrel Temperature 285 - 305 °C545 - 581 °FInjection Molding
Front Barrel Temperature 290 - 310 °C554 - 590 °FInjection Molding
Nozzle Temperature 285 - 305 °C545 - 581 °FInjection Molding
Melt Temperature 290 - 310 °C554 - 590 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °FInjection Molding
Drying Temperature 100 - 110 °C212 - 230 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPa142 - 569 psiInjection Molding
Screw Speed 40 - 70 rpm40 - 70 rpmInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency

PLAY547 / 148557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.