MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Diamond NPP30-0500 GF30 BLACK HOMOPOLYMER 30% Glass Filled Black Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Homopolymer Polypropylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Filler Content 30 %30 %Glass; ASTM D2584
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psichs 0.2 in/min; ASTM D638
Elongation at Yield 3.0 %3.0 %chs 0.2 in/min; ASTM D638
Flexural Modulus 5.27 GPa764 ksiASTM D790
Izod Impact, Notched 0.800 J/cm
@Thickness 3.17 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °F0.125";; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced
Envalior Akulon® S223-HG6 PA66-GF30, Dry, 30% Glass Filled, Heat Stabilized
A. Schulman Diamond NPP25-1503 GF30 30% Glass Filled Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 1239H Glass Filled Chemically Coupled Homopolymer Polypropylene
Aclo Accutech Polypropylene Copolymer CP0436G30CL Glass Reinforced

PDIAM405 / 126496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.