Moplen 2000HEXP is a medium fluidity heterophasic copolymer grade for injection molding applications. It exhibits an excellent impact performance, particularly at low temperature, combined with a good processability. Moplen 2000HEXP can be used in luggage, closures and it is a building block for technical compounding. It offers a good solution for interior and exterior parts in Automotive compounds. It is not intended for medical and pharmaceutical applications. The grade is available in natural, pellet form. Applications: Automotive Parts, Luggage.Information provided by LyondellBasell. |