MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DuPont Mobility and Materials Vamac® DHC Ethylene Acrylic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: DuPont™ Vamac® DHC is a dipolymer of ethylene and methylacrylate cured using peroxide vulcanization systems. This gum elastomer includes a small amount of processing aid. It has a mild acrylic odor. Use adequate ventilation during storage, mixing and processing to prevent accumulation of residual vapors. Storage stability is excellent.

Applications:Vamac® dipolymers are cured with peroxides and do not require a post cure cycle. Vamac® DHC was developed to improve the cure characteristics of the standard Vamac® dipolymer. Vamac® DHC provides for a higher state of cure and improved compression set. However, the heat age performance is impacted and slightly lower than the standard Vamac® dipolymer. Vamac® DHC is considered to be a 1500C continuous operating temperature elastomer. Vamac® DHC has better oil resistance with service lubricants exhibiting lower oil swell. Low-temperature flexibility is maintained.

Vamac® DHC would be of interest to those customers not needing the higher heat age performance of the standard Vamac® grades (1650C continuous) while wanting to maximize the properties from a non-post cure process with minimal cure time.

The properties of Vamac® DHC make it potentially suitable for a wide range of automotive applications, including powertrain seals and gaskets, rocker cover and bonded piston seals, oil coolant hoses, power steering hoses, crankcase ventilating tubes, coverings for fuel and coolant hoses, O-rings, grommets and spark plug boots. Vamac® DHC is well suited for injection, transfer and compression molding, and is easily extruded.

Information provided by DuPont™

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccnominal
Volatiles <= 0.70 %<= 0.70 %ASTM D1416
Mooney Viscosity 16.5 - 24.5
@Temperature 100 °C
16.5 - 24.5
@Temperature 212 °F
ML 1+4; ASTM D1646
Ash <= 0.20 %<= 0.20 %ASTM D1416
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262Aged for 1008 Hrs at 150°C in ASTM SF105 Oil
 7171Original
 8282Aged for 1008 Hrs at 150°C in Air
Tensile Strength at Break 15.49 MPa2247 psiAged 1008 Hrs at 150°C in ASTM SF105 Oil
 18.15 MPa2632 psiAged 1008 Hrs at 150°C in Air
 21.04 MPa3051 psiOriginal
Elongation at Break 139 %139 %Aged for 1008 Hrs at 150°C in ASTM SF105 Oil
 155 %155 %Aged for 1008 Hrs at 150°C in Air
 181 %181 %Original
100% Modulus  11.0 MPa
@Strain 100 %
1600 psi
@Strain 100 %
Original
 12.0 MPa
@Strain 100 %
1740 psi
@Strain 100 %
Aged 1008 Hrs at 150°C in Air
 13.0 MPa
@Strain 100 %
1890 psi
@Strain 100 %
Aged 1008 Hrs at 150°C in ASTM SF105 Oil
Compression Set  33.2 %
@Temperature 150 °C,
Time 605000 sec
33.2 %
@Temperature 302 °F,
Time 168 hour
in air
 50.2 %
@Temperature 150 °C,
Time 3.629e+6 sec
50.2 %
@Temperature 302 °F,
Time 1008 hour
in air
 
Descriptive Properties
Antioxidant-Naugard 445, parts1
Co-agent: HVA-2, parts2
Curative: Vulcup 40KE (peroxide), parts5
FEF black (N550)55
Release agent- Armeen 18D, parts0.5
Release agent-Stearic Acid, parts0.5
Release agent-Vanfre VAM (alkylphosphate), parts0.5
Vamac Dipolymer, parts100

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Trelleborg Vamac® E650C Ethylene-Acrylate Rubber
Arkema LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate

PDUP959 / 33526

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.