MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODASURF® ON-877 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Rhodasurf® ON 877 is Ethoxylated Oleyl Alcohol. It is excellent emulsifier, wetting agent, dispersant, and detergent

Chemical Name: ETHOXYLATED OLEYL ALCOHOL

CAS: 68526-94-3

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODASURF® ON-877 is an excellent primary nonionic surfactant, recommended especially for the emulsion polymerization of acrylic, vinyl acrylic, and styrene-acrylic polymers. Such polymers find application in latex paints, adhesives, paper coatings and textile applications. Rhodasurf ON-877 is one of a series of Rhodia nonionic surfactants with different HLBs. Since differences in HLB affect emulsification and stabilization properties, the Rhodasurf series allows the user to select the surfactant that will provide effective particle size control, low levels of coagulum, latex stability and trouble-free commercial production.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Solids Content 70 %70 %Oven
pH 6.0 - 8.06.0 - 8.010% Solution
Surface Tension 37 dynes/cm37 dynes/cm
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 4.0<= 4.0RP-0138
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 29 - 31 %29 - 31 %CME, 60% Power; RP-0528
 
Descriptive Properties
AppearancePourable, Viscous LiquidRP-0064
Cloud point63-69°C1.3% in 10% Saline, RP-0119
Critical Micelle Concentration (%)0.015
Gelation Temperature<4°C
HLB number15.4
Ionic ChargeNonionic
Neutralization Number<0.5 mg KOH/gpH 7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODASURF® ON-870 Surfactant
Solvay RHODASURF® CET 2 Surfactant
Solvay RHODASURF® LA-985 Surfactant
Solvay RHODASURF® LA-9 Surfactant
Solvay RHODASURF® LA 42 Surfactant

WRHOD452 / 137683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.