MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CMW® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten  (discontinued **)
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: This material has been rebranded as NAECOMET® 1000.

Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 16.96 g/cc0.6127 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 60
@Temperature 600 °C
60
@Temperature 1110 °F
39 HRA
Hardness, Rockwell C 2424
Tensile Strength, Ultimate 772 MPa112000 psi
Tensile Strength, Yield 517 MPa75000 psi
Elongation at Break 6.0 %6.0 %
Modulus of Elasticity 280 GPa40600 ksi
Compressive Yield Strength 683 MPa99100 psi
Fatigue Strength 276 MPa40000 psiHigh cycle unnotched
Charpy Impact 6.10 J4.50 ft-lbNotched
Charpy Impact, Unnotched 14.9 J11.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000123 ohm-cm0.0000123 ohm-cm(14% IACS)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.40 µm/m-°C
@Temperature 20.0 - 400 °C
3.00 µin/in-°F
@Temperature 68.0 - 752 °F
 6.35 µm/m-°C
@Temperature 20.0 - 800 °C
3.53 µin/in-°F
@Temperature 68.0 - 1470 °F
Thermal Conductivity 94.1 W/m-K653 BTU-in/hr-ft²-°F
Melting Point 1200 - 3410 °C2190 - 6170 °F
Solidus 1200 °C2190 °F
Liquidus 3410 °C6170 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 4.0 %4.0 %
Nickel, Ni 6.0 %6.0 %
Tungsten, W 90 %90 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® NAECOMET® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy
Aluminum 6061-T6; 6061-T651
NAECO® NAECOMET® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
NAECO® NAECOMET® 3970 AMS-T-21014 ASTM B777 High Density Machinable Tungsten

NCMW02 / 15874

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.