MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Montmorillonite - Smectite ((Na,Ca)(Al,Mg)6(Si4O10)3(OH)6-nH2O)
Categories: Ceramic; Clay

Material Notes: Description: A clay mineral having a 2:1 expanding crystal lattice. Isomorphous substitution gives the various types and causes a net permanent charge balanced by cations in such a manner that water may move between the sheets, giving reversible cation exchange and very plastic properties. Crystals expand to many times their volume when added to water.
Uses: Used to slow the progress of water through soil or rocks; Used in drilling muds to give the water greater viscosity; Used to produce nanocomposites: Used as an absorbent to purify and decolor liquids; Used as a filler in paper and rubber; and used as a base for cosmetics and medicines. Forms Available: Powder

Information provided by Reade Advanced Materials.

Key Words: (Na,Ca) (Al,Mg)6(Si4O10)3(OH)6-nH20, Montmorillonite, Smectite, Sodium montmorillonite (Sodium bentonite (Wyoming bentonite (US)), Swelling bentonite (Western bentonite (US), Sodium-activated bentonite (Bentonitte (UK)), Sodium-exchanged bentonite, (Synthetic bentonite)), Calcium montmorillonite (Calcium bentonite (Mississippi bentonite (US)), Sub-bentonite (Texas bentonite (US)), Magnesium montmorillonite (Saponite & Armargosite), Potassium montmorillonite (Metabentonite), and Lithium montmorillonite (Hectorite))
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 - 3.00 g/cc2.30 - 3.00 g/cc
Density 2.350 g/cc0.08490 lb/in³
Molecular Weight 540.46 g/mol540.46 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 1.5 - 2.01.5 - 2.020°C
 
Descriptive Properties
Colorwhite, yellow
Crystal Structuremonoclinic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 385 S Polyurethane
Covestro Desmopan® 385 Thermoplastic Polyurethane
Potassium Carbonate Sesquihydrate, K2CO3-1.5H2O
Potassium Carbonate, K2CO3
Reade Advanced Materials Bentonite Powder (BaTiSi3O9)

CREADE018 / 1952

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.