MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Hifor Clear SC74580 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: WESTLAKE Hifor Clear Polyethylene SC74580 polymer is a high strength and high clarity linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock. It does contain processing aid. Blown films produced with this resin exhibit good toughness, with exceptional gloss and clarity for a product of this density, yet film blocking is substantially lower than one might expect. Film stiffness is also higher than one might expect for this density. It works well in many shrink film applications. Contact Westlake for further information on the regulatory status.

    Application/Uses
  • Frozen food films
  • High clarity bread bags
  • Ice bags

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Good toughness, with exceptional gloss and clarity
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil
Melt Flow 0.60 g/10 min0.60 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 600 %600 %ASTM D882
Film Elongation at Break, TD 950 %950 %ASTM D882
Dart Drop 3.94 g/micron100 g/milASTM D1709
Film Tensile Strength at Break, MD 56.5 MPa8200 psiASTM D882
Film Tensile Strength at Break, TD 37.9 MPa5500 psiASTM D882
1% Secant Modulus, MD 324 MPa47000 psiASTM D882
1% Secant Modulus, TD 379 MPa55000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
Gloss 82 %82 %at 45º; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 216 °C400 - 420 °F
Blow-up Ratio (BUR) 2.42.4
 
Descriptive Properties
ProcessBlown Film
 Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Hifor Clear SC74558 Linear Low Density Polyethylene
Westlake EMAC® SP2409 20% EMA Copolymer
Westlake EC1390AA Low Density Polyethylene
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade

PWESF118 / 84555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.