System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Durethan® BKV 35 XTS1 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 40% Glass Fiber Filled
Material Notes:
PA 6, 35% glass fibers, injection molding, heat-aging stabilized, notably high heat-aging stability
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.41
g/cc
0.0509
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0023
cm/cm
0.0023
in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0073
cm/cm
0.0073
in/in
60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
180
MPa
26100
psi
5 mm/min; ISO 527-1,-2
Elongation at Break
3.0 %
3.0 %
Nominal, 50 mm/min; ISO 527-1,-2
Tensile Modulus
10.7
GPa
1550
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
270
MPa
39200
psi
2 mm/min; ISO 178-A
Flexural Modulus
10.4
GPa
1510
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
3.4 %
3.4 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
10.0
kJ/m²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
70.0
kJ/m²
@Temperature 23.0 °C
33.3
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
7.00
J/cm²
@Temperature 23.0 °C
33.3
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
0.800
J/cm²
@Temperature -30.0 °C
3.81
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
1.00
J/cm²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
17.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
9.44
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow
100
µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point
221
°C
430
°F
10°C/min; ISO 11357-1,-3
Deflection Temperature at 1.8 MPa (264 psi)
205
°C
401
°F
ISO 75-1,-2
Shrinkage, MD
0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.30 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Processing Properties
Metric
English
Comments
Melt Temperature
250
-
290
°C
482
-
554
°F
280
°C
536
°F
injection molding
Mold Temperature
80.0
°C
176
°F
injection molding
80.0
-
100
°C
176
-
212
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
6.00
hour
2.00
-
6.00
hour
Moisture Content
0.030 - 0.12 %
0.030 - 0.12 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Durethan® BKV 35 H2.0 901510 Nylon 6 (PA6), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® BKV 30 XTS1 901510 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 35 XTS1 901510 Nylon 66 (PA66), 35% Glass Fiber Reinforced, Dry
Envalior Durethan® AKV 35 HR H2.0 901510 Nylon 66 (PA66), 35% Glass Fiber Reinforced, Conditioned
Envalior Durethan® AKV 30 XTS1 901510 Nylon 66 (PA66), 30% Glass Fiber Reinforced, Dry
PLANW9412 / 208243
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.