MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® HFX 33 PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and enhanced heat stability.

Applications: Ultramid HFX 33 is recommended for tubing applications requiring an outstanding balance of flexibility, chemical and heat resistance and burst performance.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 38.0 MPa5510 psiISO 527
Elongation at Break 160 %160 %Nominal; ISO 527
Tensile Modulus 0.494 GPa71.6 ksiISO 527
Flexural Modulus 0.480 GPa69.6 ksiISO 178
Izod Impact, Notched (ISO) 101 kJ/m²48.1 ft-lb/in²ISO 180
Charpy Impact, Notched 11.7 J/cm²55.7 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C104 °FISO 75
 
Processing PropertiesMetricEnglishComments
Zone 1 225 - 245 °C437 - 473 °FRear
Zone 2 225 - 250 °C437 - 482 °FMiddle
Zone 3 225 - 245 °C437 - 473 °FFront
Zone 4 230 - 245 °C446 - 473 °FHead
Zone 5 230 - 245 °C446 - 473 °FFlange
Die Temperature 230 - 245 °C446 - 473 °F
Melt Temperature 225 - 245 °C437 - 473 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Renol PA111G35IF Nylon 66, 35% Glass Fiber, Improved Flow
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Conditioned)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry)

PBASG0443 / 132076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.