MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ferro Zirmonite 1000, TZP
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: TZP, ZrO2, zirconia, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.05 g/cc0.219 lb/in³
Water Absorption 0.00 %0.00 %
Open Porosity 0.00 %0.00 %Gas tight. Test with helium mass spectrometer
Weibull Modulus 1919
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 10351035KHN5 microhardness, kg/mm²
Vickers Microhardness 11501150HV5 microhardness, kg/mm²
Tensile Strength, Ultimate 584 MPa84700 psiACMA Test #4
Modulus of Elasticity 172 GPa24900 ksiultrasonic
Compressive Strength 2930 MPa425000 psiASTM C773-74
Poissons Ratio 0.330.33ASTM C623
Fracture Toughness 12.0 MPa-m½10.9 ksi-in½Kic (indentation)
Shear Modulus 75.8 GPa11000 ksiultrasonic
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.90 µm/m-°C
@Temperature 25.0 - 200 °C
3.28 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM C32
 9.90 µm/m-°C
@Temperature 25.0 - 500 °C
5.50 µin/in-°F
@Temperature 77.0 - 932 °F
ASTM C32
 10.7 µm/m-°C
@Temperature 25.0 - 800 °C
5.94 µin/in-°F
@Temperature 77.0 - 1470 °F
 10.9 µm/m-°C
@Temperature 25.0 - 1000 °C
6.06 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C32
Thermal Conductivity 2.90 W/m-K20.1 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorGold

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MMCC Al/B4C Particulate Aluminum Matrix Composite
ICE ZrO
Morgan Advanced Ceramics Nilcra® Zirconia MS Grade Zirconia
Ferro Zirmonite 200, ZTA
Morgan Advanced Ceramics Nilcra® Zirconia TS Technical Ceramic

CFC014 / 812

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.