MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NOVA Chemicals Sclair® SD-7250-0B HDPE Extrusion Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Good adhesion, Excellent barrier properties, Good heat resistance

Applications: Silicon-coated release papers, Composite can liners, Base coat for photographic papers, Snack food packaging

Additives: Antioxidant

Heat Seal Temperature: 135°C , minimum value, 1-mil coating on kraft paper

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³ASTM D792
Moisture Vapor Transmission 0.305 cc-mm/m²-24hr-atm0.775 cc-mil/100 in²-24hr-atm1 mil coating on kraft paper; ASTM F1249-89
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In 5.00 cm1.97 inNeck in reported is the total of both sides
Drawdown 8.10 m/s1590 ft/min
Coating Weight >= 10.4 g/m²>= 6.50 lb/ream
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.200.20Gloss coating, Film to metal; ASTM D1894
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °F
Vicat Softening Point 117 °C243 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Novapol® HE-Y449-AC HDPE Extrusion Resin
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion)
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion)
LyondellBasell Petrothene® LR734001 High Density Polyethylene, Sheet & Profile Extrusion Data
LyondellBasell Alathon® H6018 High Density Polyethylene (Extrusion Grade)

PNOVA141 / 55042

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.