MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxygen-free extra-low phosphorus Copper, UNS C10300, H80 (40%) temper, rod, tube
Categories: Metal; Nonferrous Metal; Copper Alloy; Wrought Copper

Material Notes: Test specimens: rod - 6 mm diam.; tubing - 25 mm OD, 1.65 mm thick.

Applications: electrical conductors and terminals, tubular busbars, commutators, copper clad steel and clad products, waveguide tubing, thermostatic control tubing, and applications requiring good conductivity and welding or brazing properties.

Processing: Excellent hot and cold workability; good forgeability. Annealing temp.: 475-750°C (900-1400°F). Hot working temp.: 750-875°C (1400-1600°F). Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Corrosion Resistance: Good to excellent

Weldability: excellent welding and brazing properties.

UNS C10300, CDA 103, ASTM (rod) B12, B133, B187, (tubing) B68, B75, B88, B111, B188, B251, B280, B306, B359, B372, B395, B447

Key Words: ASTM B280, 306, 359, 372, 395, 447, OFXLP, CDA 103, ASTM B68, 75, 88, 111, 133, 187, 188, 251
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6060
Hardness, Rockwell F 9494Rod
 95
@Diameter 25.0 mm
95
@Diameter 0.984 in
tubing
Hardness, Rockwell 30T 6363Tubing
Tensile Strength, Ultimate 380 MPa55100 psi
Tensile Strength, Yield 345 MPa50000 psi
Elongation at Break 20 %20 %in 50 mm (2 in.), rod
 8.0 %
@Diameter 25.0 mm
8.0 %
@Diameter 0.984 in
tubing
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.310.31
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 200 MPa29000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000174 ohm-cm
@Temperature 20.0 °C
0.00000174 ohm-cm
@Temperature 68.0 °F
99% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 386 W/m-K
@Temperature 20.0 °C
2680 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1083 °C1981 °F
Solidus 1083 °C1981 °F
Liquidus 1083 °C1981 °F
Annealing Point >= 371 °C>= 700 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99.95 %99.95 %Includes Cu+Ag+P
Other <= 0.050 %<= 0.050 %
Phosphorus, P 0.0010 - 0.0050 %0.0010 - 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free extra-low phosphorus Copper, UNS C10300, H80 (15%) temper, tube, shapes
Oxygen-free extra-low phosphorus Copper, UNS C10300, OS050 temper, flat products, tube, and shapes
Oxygen-free extra-low phosphorus Copper, UNS C10300, OS025 temper, flat products, tube
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products
AISI 1020 Steel, as rolled

MC10300c4 / 10391

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.