MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reliance Industries 57-01 Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Information provided by Reliance Industries

Applications: Rigid injection.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.480 - 0.540 g/cc0.0173 - 0.0195 lb/in³PVCH/QCD/3516
Particle Mesh Size 40 Mesh40 MeshTraces; PVCH/QCD/3514
 60 Mesh60 Mesh5% Retention; PVCH/QCD/3514
 140 Mesh140 Mesh50% Retention; PVCH/QCD/3514
Collected Volatile Condensable Material <= 0.00030 %<= 0.00030 %PVCH/QCD/3520
 
Descriptive Properties
Fish Eye count, No. 20RILH/QA(P)/3782
Heat Loss, %(max.)0.3PVCHQCD/3513
K-Value57PVCH/QCD/3512; 1% in cyclohexanone at 30°C
Porosity DOP Absorption, ml/g0.24-0.36PVCH/QCD/3515

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reliance Industries Polypropylene Impact Copolymer
Reliance Industries 67-01 Polyvinyl Chloride
Mitsubishi Iupital® ET-25 Copolymer Acetal
Reliance Industries Repol B030MG Polypropylene
Reliance Industries Polypropylene Random Copolymer

PREL085 / 65425

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.