MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 1015 Steel, annealed at 870°C (1600°F)
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Better machinability and carburizing. Can be strengthened by cold working or surface hardened by carburizing or cyaniding. Hot rolled sheet has excellent weldability.

Key Words: UNS G10150, AISI1015, AMS 5060, ASTM A29, ASTM A108, ASTM A510, ASTM A545, ASTM A549, ASTM A575, ASTM A576, ASTM A659, FED QQ-S-698 (C1015), MIL SPEC MIL-S-16974, SAE J403, JIS S 17 C, JIS S 15 CK, SS14 1370 (Sweden), SAE J412, SAE J414, DIN 1.1141, AFNOR XC 15 (Fr), AFNOR XC 18 (Fr), JIS S 15 C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 111111
Hardness, Knoop 129129Converted from Brinell
Hardness, Rockwell B 6464Converted from Brinell
Hardness, Vickers 115115Converted from Brinell
Tensile Strength, Ultimate 385 MPa55800 psi
Tensile Strength, Yield 285 MPa41300 psi
Elongation at Break 37 %37 %in 50 mm
Reduction of Area 70 %70 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Machinability 60 %60 %Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
Izod Impact 115 J84.8 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000159 ohm-cm
@Temperature 0.000 °C
0.0000159 ohm-cm
@Temperature 32.0 °F
annealed condition
 0.0000219 ohm-cm
@Temperature 100 °C
0.0000219 ohm-cm
@Temperature 212 °F
annealed condition
 0.0000292 ohm-cm
@Temperature 200 °C
0.0000292 ohm-cm
@Temperature 392 °F
annealed condition
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.9 µm/m-°C
@Temperature 0.000 - 100 °C
6.61 µin/in-°F
@Temperature 32.0 - 212 °F
 12.4 µm/m-°C
@Temperature 0.000 - 200 °C
6.89 µin/in-°F
@Temperature 32.0 - 392 °F
 13.0 µm/m-°C
@Temperature 0.000 - 300 °C
7.22 µin/in-°F
@Temperature 32.0 - 572 °F
 13.5 µm/m-°C
@Temperature 0.000 - 400 °C
7.50 µin/in-°F
@Temperature 32.0 - 752 °F
 14.2 µm/m-°C
@Temperature 0.000 - 500 °C
7.89 µin/in-°F
@Temperature 32.0 - 932 °F
Specific Heat Capacity  0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
 0.519 J/g-°C
@Temperature 150 - 200 °C
0.124 BTU/lb-°F
@Temperature 302 - 392 °F
 0.599 J/g-°C
@Temperature 350 - 400 °C
0.143 BTU/lb-°F
@Temperature 662 - 752 °F
Thermal Conductivity  48.9 W/m-K
@Temperature 200 °C
339 BTU-in/hr-ft²-°F
@Temperature 392 °F
Annealed
 51.0 W/m-K
@Temperature 100 °C
354 BTU-in/hr-ft²-°F
@Temperature 212 °F
Annealed
 51.9 W/m-K
@Temperature 0.000 °C
360 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
Annealed
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.13 - 0.18 %0.13 - 0.18 %
Iron, Fe 99.13 - 99.57 %99.13 - 99.57 %As remainder
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1015 Steel, normalized at 925°C (1700°F)
AISI 1015 Steel, cold drawn
AISI 1015 Steel, as rolled
AISI 1015 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1015 Steel, annealed at 870°C (1600°F), furnace cooled 17°C (31°F) per hour to 725°C (1340°F), air cooled, 25 mm (1 in.) round

M1015F / 6795

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.