MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Elastosil® LR 3074/60 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product description: Self-adhesive liquid silicone rubber ELASTOSIL® LR 3074/60 A/B is a paste-like, easily-pigmentable two component compound with extremely short curing times and improved coolant resistance.

Special features: ELASTOSIL® LR 3074/60 A/B is a primerless, self bonding grade that adheres to various plastic substrates (e. g. PA, PBT) and metals, but not in the mold. The bonding is improved by an ageing-process (e. g. one hour at 100 °C) or by a longer storing at room temperature. Because of the individual surface properties each substrate must be tested before mass production. The vulcanizates are opaque and noted for average mechanical and electrical properties.

Application: ELASTOSIL® LR 3074/60 A/B is particularly suitable for the economical production of large series of overmolded parts (thermoplastic/elastomer), which are used for radiator in the automotive industry. Parts made from ELASTOSIL® LR 3074/60 A/B can generally be used for technical applications without post-curing, but do not comply with regulations concerning use in the pharmaceutical and food industries.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-1 A
Viscosity  270000 cP
@Shear Rate 10.0 1/s
270000 cP
@Shear Rate 10.0 1/s
DIN 53019
 1.20e+6 cP
@Shear Rate 0.900 1/s
1.20e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858DIN 53505
Tensile Strength at Break 6.80 MPa986 psiDIN 53504 S 1
Elongation at Break 360 %360 %DIN 53504 S 1
Rebound 65 %65 %DIN 53512
Tear Strength 16.0 kN/m91.3 pliASTM 624 B
Compression Set  15 %
@Temperature 125 °C,
Time 79200 sec
15 %
@Temperature 257 °F,
Time 22.0 hour
DIN ISO 815-B
 21 %
@Temperature 150 °C,
Time 79200 sec
21 %
@Temperature 302 °F,
Time 22.0 hour
DIN ISO 815-B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °Fwith heat stabilizer
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
in press
 
Descriptive Properties
Appearanceopaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/70 A/B Liquid Silicone Rubber
304 Stainless Steel
Dow Silastic® RBL-9200-70 LSR Liquid Silicone Rubber
Dow Silastic® RBL-9200-60 LSR Liquid Silicone Rubber
Wacker Elastosil® LR 3003/70 W A/B Liquid Silicone Rubber

PWACK9145 / 204674

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.