MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 104 CC FR A Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - Non PBB/PBDE
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D 792
Water Absorption 0.030 %
@Time 86400 sec
0.030 %
@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage 0.0015 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0015 - 0.0030 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 2.0 - 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 - 4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D 785
Tensile Strength at Break 68.9 MPa10000 psiASTM D 638
Elongation at Break 2.5 - 4.0 %2.5 - 4.0 %ASTM D 638
Tensile Modulus 6.89 GPa1000 ksiASTM D 638
Flexural Strength 114 MPa16500 psiASTM D 790
Flexural Modulus 6.07 GPa880 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.20 mm
2.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmESD STM11.11
Dielectric Constant 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 23.6 kV/mm600 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
Dry; ASTM D 150
Arc Resistance 85 sec85 secASTM D 495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C315 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FASTM D 648
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 232 °C375 - 450 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 104 CC FR A UV Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - Non- PBB/PBDE - UV Stabilized
RTP Company RTP 107 CC Polypropylene (PP), Glass Fiber - Chemically Coupled
ExxonMobil Santoprene® 241-73 Thermoplastic Elastomer
RTP Company RTP 105 CC FR Polypropylene (PP), Glass Fiber - Chemically Coupled - Flame Retardant - UL94 V-0
304 Stainless Steel

PQZTA12754 / 159189

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.