MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Chemours Viton® ETP-900  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® Extreme™ ETP-600S (developmental product VTR-8710) is a new specialty fluoroelastomer, built on DuPont Dow's proprietary Advanced Polymer Architecture (APA) technology, that provides the excellent end-use performance of Viton® Extreme™ ETP-900 with significant improvements in processing and cure characteristics. The APA technology upgrades the peroxide cure site and optimizes the molecular structure to deliver a polymer which:
  • Cures faster, and to a higher state of cure, than Viton® Extreme™ ETP-900
  • Provides excellent mold release and low mold fouling
  • Exhibits better mold flow and less shear sensitivity
  • Has improved compression set resistance when compared to ETP-900
  • Gives the same broad fluid and heat resistance of other Viton® Extreme™ ETP polymers

Viton® Extreme™ ETP-600S takes specialty fluoroelastomer performance to a new level of processing ease combined with the excellent end-use performance.

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 81
@Temperature 121 °C
81
@Temperature 250 °F
ML 1 + 10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777Cured 7 min at 177°C and Post Cured 16 hr at 200°C
Tensile Strength, Ultimate 17.3 MPa2510 psiCured 7 min at 177°C and Post Cured 16 hr at 200°C
Elongation at Break 213 %213 %Cured 7 min at 177°C and Post Cured 16 hr at 200°C
50% Modulus 3.60 MPa
@Strain 50 %
3.60 MPa
@Strain 50 %
Cured 7 min at 177°C and Post Cured 16 hr at 200°C
100% Modulus 8.80 MPa
@Strain 100 %
1280 psi
@Strain 100 %
Cured 7 min at 177°C and Post Cured 16 hr at 200°C
Compression Set 49 %
@Temperature 200 °C
49 %
@Temperature 392 °F
Method B, O-rings 70 hr at 200°C (Post Cured 16 hr at 232°C)
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -6.00 °C21.2 °FTR-10
Glass Transition Temp, Tg -11.0 °C12.2 °FMDSC
 
Descriptive Properties
Formulation as Tested100Viton® Extreme™ ETP-900
 3Zinc Oxide
 3Diak™ 7 (TAIC)
 3Luperox® 101XL45
 30N990 Carbon Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® ETP-500 Fluoroelastomer (FKM)
Chemours Viton® B-70 Fluoroelastomer (FKM), Low Temperature Grade
Chemours Viton® F-605C Fluoroelastomer Compound
Chemours Viton® GF300
Chemours Viton® A-200 Fluoroelastomer Compound

PDVDA63 / 34032

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.