MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aperam Supera 50/50sp Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: SUPRA50 /SUPRA50SP is an iron-nickel soft magnetic alloys with maximum saturation induction and high permeability. Main applications are relays, gas safety, sensors, watches, shieldings.

International standards: ASTM A 753, DIN 17405, IEC 404, JIS C 2531

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 140140Annealed
 250250Hard Temper
Tensile Strength 500 MPa72500 psiAnnealed
 700 MPa102000 psiHard Temper
Tensile Strength, Yield 280 MPa40600 psiAnnealed
 1030 MPa149000 psiHard Temper
Elongation at Break 3.0 %3.0 %Hard Temper
 35 %35 %Annealed
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000045 ohm-cm0.0000045 ohm-cm
Magnetic Permeability  12500
@Thickness 0.350 mm
12500
@Thickness 0.0138 in
AC
 <= 200000
@Thickness 0.350 mm
<= 200000
@Thickness 0.0138 in
DC
Magnetic Coercive Force, Hc 0.035 Oe
@Thickness 0.350 mm
0.035 Oe
@Thickness 0.0138 in
DC
Magnetic Saturation Flux Density, Bmax  15000 Gauss
@Thickness 0.350 mm
15000 Gauss
@Thickness 0.0138 in
DC, Saturation Induction
 15000 Gauss
@Thickness 0.350 mm
15000 Gauss
@Thickness 0.0138 in
AC, Saturation Induction
Curie Temperature 450 °C842 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 µm/m-°C7.22 µin/in-°F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K90.2 BTU-in/hr-ft²-°F
Melting Point 1425 °C2597 °F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 52 %52 %
Nickel, Ni 48 %48 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aperam Permimphy Cold Rolled Strip
Aperam Mumetal Cold Rolled Strip
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
Aperam Supera 50T Cold Rolled Strip
Aperam Supermimphy® LLS Cold Rolled Strip

NPERA015 / 194804

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.