MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Heraeus Clevios™ PH Conductive Sulfonate Polymer for Antistatic Coatings
Categories: Polymer

Material Notes: Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Clevios™ PH is an antistatic material based on PEDOT:PSS – chemistry for electronics applications. This conductive polymer is a homogenized version of Clevios™ P with a very high transmission in the visible spectrum and a mean particle size – d50 approx. 30 nm (swollen).

Typical applications include the antistatic coating of PET or Polycarbonate films for antistatic trays and blister tapes, films for dust protection of components in the LCD industry, antistatic coating of glass, high quality antistatic-coated papers, and other ESD and dissipative applications

Application Methods: Dipping, Spraying, Printing (including gravure, slot-die)

Information provided by Heraeus, Conductive Polymers Division.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.003 g/cc
@Temperature 20.0 °C
0.03624 lb/in³
@Temperature 68.0 °F
Solids Content 1.2 - 1.4 %1.2 - 1.4 %As Supplied
Particle Size 0.030 µm0.030 µmD50 swollen
pH 1.5 - 2.51.5 - 2.5As Supplied
Viscosity 10 - 30 cP10 - 30 cPAs Supplied
Surface Tension 71 dynes/cm
@Temperature 20.0 °C
71 dynes/cm
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 - 0.100 ohm-cm0.0100 - 0.100 ohm-cmApplied Coating; formulated with DMSO or MEG
Surface Resistivity per Square 1.00e+6 ohm1.00e+6 ohmApplied Coating
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5228
@Wavelength 589 nm
1.5228
@Wavelength 589 nm
Transmission, Visible >= 90 %
@Thickness 0.000100 mm
>= 90 %
@Thickness 0.00000394 in
Applied Coating
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month
@Temperature 20.0 °C
9.00 Month
@Temperature 68.0 °F
in unopened original container
 
Descriptive Properties
Form SuppliedLiquid
OdorNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Heraeus Clevios™ P T2 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P Jet N V2 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P Jet 700 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ S HT Antistatic/Conductive Polymer Coating for Screen Printing

PHERA991 / 149955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.