MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Stat-Rite® S-250 Static Control Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite IDP alloys provide consistent static dissipation even when extruded, injection molded, or thermoformed into components.

Features:

  • Permanently static dissipative
  • Humidity insensitive
  • Ultra-Clean: low off-gassing, low ionic contamination
  • Colorable
  • Durable: Can be used repeatedly.

Applications:

  • Semiconductor handling
  • Medical device packaging
  • Electronic component handling
  • Disk packaging
  • Cleanroom supplies

Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.9 MPa3900 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Tensile Modulus 1.28 GPa185 ksiASTM D638
Flexural Modulus 1.28 GPa185 ksiASTM D790-90
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256-92
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+10 ohm-cm3.00e+10 ohm-cm50% RH; ASTM D257
Surface Resistance 8.00e+8 ohm8.00e+8 ohmESD S11.11; 12 % R.H.
Surface Resistivity per Square 8.00e+9 ohm8.00e+9 ohm50% RH; ASTM D257
Static Decay 0.010 sec0.010 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 0.010 sec0.010 secFTMS-101C; 12% R.H., (-5000 V to -50 V)
 0.50 sec0.50 secCharged Plate Monitor; 50% R.H.
Tribocharge 10 V10 VNitrile Glove - BFG Test Method
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FASTM D648
 
Descriptive Properties
ColorLight Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer
Lubrizol STAT-RITE® E-1140 Ester-Type Static Dissipative Polymer
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene

PNOVEON22 / 55454

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.