MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 4099 X 105534 Polyphthalamide (PPA), Wear Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 172 MPa25000 psiASTM D 638
Elongation at Break 1.5 - 3.0 %1.5 - 3.0 %ASTM D 638
Tensile Modulus 12.1 GPa1750 ksiASTM D 638
Flexural Strength 248 MPa36000 psiASTM D 790
Flexural Modulus 9.65 GPa1400 ksiASTM D 790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.17 mm
0.800 ft-lb/in
@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 3.74 J/cm
@Thickness 3.17 mm
7.00 ft-lb/in
@Thickness 0.125 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+6 ohm-cm<= 1.00e+6 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 302 - 329 °C575 - 625 °F
Mold Temperature 135 - 163 °C275 - 325 °F
Drying Temperature 107 °C
@Time 14400 - 21600 sec
225 °F
@Time 4.00 - 6.00 hour
Moisture Content 0.050 %0.050 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 4099 X 130514 D Polyphthalamide (PPA) Glass Fiber - Flame Retardant - Halogen Free
RTP Company RTP 4099 X 128641 A Polyphthalamide (PPA), Thermally Conductive - Electrically Insulative - Preliminary Datasheet
RTP Company RTP 4099 X 128640 Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive - Preliminary Datasheet
RTP Company RTP 4099 X 123510 A Polyphthalamide (PPA), Carbon Fiber - Aramid Fiber - Impact Modified - PTFE Lubricated - Silicone Lubricated
LNP Lubricomp® WFL-4036 Polybutylene Terephthalate, Glass Fiber Reinforced, PTFE Lubricant

PQZTA4511 / 159207

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.