MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers Elix™ 260 P SAN Polymer Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; SAN Polymer

Material Notes: High flow SAN copolymer- powder version. Employed to improve flow ability and thermoforming properties of PVC compounds. Used as base resin in color concentrates. Can be blended with high rubber modifiers to manufacture or modify properties profile of ABS resin and blends containing Polycarbonate. Improved flow ability for ABS grades. Superior dimensional stability and heat resistance for PVC compounds. Easy dispersion for pigments and colorants. Physical form: white powder.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 125 - 650 µm125 - 650 µm>90%; ASTM D1921
Melt Flow 50 - 61 g/10 min
@Load 10.0 kg,
Temperature 220 °C
50 - 61 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min MVR; ISO 1133
 
Descriptive Properties
Acrylonitrile Content26.5-28.5%lab internal-IR
Base Colormax. 70DIN 6271 (20% solution in DMF)
Residual Styrene< 600 ppmlab internal-GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® WSF-1121 Foam
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced
Lucite International Elvacite® 2552 Acrylic Resin

PELIX935 / 192529

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.