MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramabind™ 830 High Temperature Inorganic Binder
Categories: Ceramic

Material Notes: A basic solution compatible with most oxide and metal powders. Ideal for formulating high pigment-to-binder ratios to produce dense adhesives and coatings. Sets at room temperature to a moisture resistant film and does not require a heat cure. Use only for thin coating systems less than 1 mil thick.

Key Words: Coatings
Vendors: Aremco’s Ceramabind materials are unique binder systems used to formulate adhesives, coatings and potting compounds for applications to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Solids Content 25 %25 %by weight
pH 11.411.4
Viscosity 10 cP10 cP
Storage Temperature 7.22 - 35.0 °C45.0 - 95.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1090 °C2000 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 0.5 hour0.5 hourair dry
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramabind™ 880 High Temperature Inorganic Binder
Aremco Ceramabind™ 875 High Temperature Inorganic Binder
Aremco Ceramabind™ 644-S High Temperature Inorganic Binder
Aremco Ceramabind™ 644-A High Temperature Inorganic Binder
Aremco Ceramabind™ 643-2 High Temperature Inorganic Binder

CAREM84 / 625

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.