MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°F. Electrode slag remelting is employed to assure preferred ingot solidification and superior cleanliness for critical applications.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.76 g/cc7.76 g/cc
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1300 - 1300 MPa188000 - 189000 psi
Tensile Strength, Yield 1041 - 1048 MPa
@Strain 0.2 %
151000 - 152000 psi
@Strain 0.2 %
Elongation at Break 18 - 19 %18 - 19 %% in 4D
Reduction of Area 60 - 63 %60 - 63 %
Modulus of Elasticity 213 GPa30900 ksi
 170 GPa
@Temperature 538 °C
24600 ksi
@Temperature 1000 °F
 199 GPa
@Temperature 260 °C
28800 ksi
@Temperature 500 °F
Notched Tensile Strength 2116 - 2130 MPa306900 - 309000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.2 µm/m-°C
@Temperature 20.0 - 260 °C
6.22 µin/in-°F
@Temperature 68.0 - 500 °F
 12.1 µm/m-°C
@Temperature 20.0 - 538 °C
6.72 µin/in-°F
@Temperature 68.0 - 1000 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.14 %0.14 %
Chromium, Cr 12 %12 %
Iron, Fe 82.175 %82.175 %
Manganese, Mn 0.70 %0.70 %
Molybdenum, Mo 1.75 %1.75 %
Nickel, Ni 2.75 %2.75 %
Nitrogen, N >= 0.035 %>= 0.035 %
Silicon, Si 0.15 %0.15 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal
410 Stainless Steel
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel
Latrobe Lescalloy® BG42 VIM-VAR High Performance Bearing Steel
AK Steel 410 Martensitic Stainless steel

NTIMK059 / 19406

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.