MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Durethan® DP 1803/10 H3.0 000000 Nylon 6 (PA6), 50% Glass/Mineral Reinforced, Flame Retardant, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant; Nylon 6, Glass/Mineral Reinforced

Material Notes: 50% glass fibers and mineral, UL94V-2 (0.75 mm)

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in150x105x3; ISO 2577
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 194 MPa28100 psiISO 2093-1
Tensile Strength at Break 107 MPa15500 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.3 %2.3 %5 mm/min; ISO 527-1,-2
Tensile Modulus 8.50 GPa1230 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 180 MPa26100 psi2 mm/min; ISO 178-A
Flexural Modulus 8.00 GPa1160 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 3.1 %3.1 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
22.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 223 °C433 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 168 °C334 °FISO 75-1,-2
Flammability, UL94 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
1430 °F
@Thickness 0.118 in
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
Shrinkage, MD 0.13 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.13 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
Shrinkage, TD 0.11 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.11 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 2577
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °F
Mold Temperature 80.0 °C176 °F
Back Pressure 60.0 MPa8700 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo GLAMIDE® T-802 Nylon-6
Envalior Durethan® DP 1803/10 H3.0 000000 Nylon 6 (PA6), 50% Glass/Mineral Reinforced, Flame Retardant, Conditioned

PLANW9581 / 208319

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.