MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom™ 63A6-4 Polypropylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Calcium Carbonate (CaCO3) Filler

Material Notes: Description: Hostacom™ 63A6-4 medium high melt flow, 2,200 MPa flexural modulus, 40% calcium carbonate-filled polypropylene homopolymer has an excellent combination of properties, chemical resistance, aesthetics and processability. Uses: lawn and garden equipment, housings, consumer applications

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9696ASTM D 785
Tensile Strength at Break 18.0 MPa2610 psiASTM D 638
Tensile Strength, Yield 23.0 MPa3340 psiASTM D 638
Elongation at Break 90 %90 %ASTM D 638
Elongation at Yield 4.0 %4.0 %ASTM D 638
Flexural Modulus 2.20 GPa319 ksiTangent, 0.05 in/min; ASTM D790
Izod Impact, Notched 0.368 J/cm0.690 ft-lb/in73°F; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C201 °FUnannealed; ASTM D648
UL RTI, Electrical  221 °C
@Thickness 1.50 mm
430 °F
@Thickness 0.0590 in
UL 746
 221 °C
@Thickness 3.00 mm
430 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  221 °C
@Thickness 1.50 mm
430 °F
@Thickness 0.0590 in
UL 746
 221 °C
@Thickness 3.00 mm
430 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  221 °C
@Thickness 1.50 mm
430 °F
@Thickness 0.0590 in
UL 746
 221 °C
@Thickness 3.00 mm
430 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ 62F4-2C Polypropylene Homopolymer
LyondellBasell Hostacom™ AE716BC Polypropylene Homopolymer
LyondellBasell Astryn SB572C Polypropylene Copolymer
LyondellBasell Hostacom™ BC142/1AC Polypropylene Copolymer
LyondellBasell Hostacom™ 6551 Polypropylene Homopolymer

PMO805 / 53794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.