MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUTENE LB4500 LDPE Extrusion Coating  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Description: LUTENE LB4500 is mainly intended for extrusion coating and can be processed uniform thickness and width. LUTENE LB4500 is also noted for the excellent heat stability and has good silicone coating processability. LB4500 has a good adhesion strength with paper and paper board and excellent neck-in characteristic. LUTENE LB4500 contains no additives.

Main Application: Release paper, kraft paper, paper cup

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.918 g/cc0.918 g/ccASTM D1505
Water Vapor Transmission 20.0 g/m²/day
@Pressure 0.101 MPa
1.29 g/100 in²/day
@Pressure 14.7 psi
ASTM D393
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444ASTM D2240
Tensile Strength at Break 13.0 MPa1890 psi200mm/min; ASTM D638
Tensile Strength, Yield 9.32 MPa1350 psi200 mm/min; ASTM D638
Elongation at Break 540 %540 %200 mm/min; ASTM D638
Flexural Modulus 0.196 GPa28.4 ksi200mm/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 107 °C225 °F10°C/min; DSC

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUTENE FB0300 LDPE Blown Film Grade
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Borealis CA7230 Low Density Polyethylene
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin

PLAY216 / 148226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.