MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Triplex Annealed Sheet
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: High-Strength, Intermediate Temperature Alloy. TIMETAL 6-2-4-6 is a stronger derivative of TIMETAL 6-2-4-2 offering higher strength, depth hardenability and elevated temperature properties up to 450°C. This alloy is similar in forgeability and crack sensitivity to TIMETAL 6-4. This alloy is used in intermediate compressor stages of turbine engines for disks and blades, seals, and for airframe parts. It is nonmagnetic.

Mechanical property data for sample after 855°C/15min/FAC + 730 °C/15min/AC + 595°C/2hr/AC triplex anneal treatment.

Data provided by TIMET.

Key Words: UNS R56260
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.64 g/cc0.168 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  200 MPa
@Temperature 750 °C
29000 psi
@Temperature 1380 °F
 780 MPa
@Temperature 600 °C
113000 psi
@Temperature 1110 °F
 1200 MPa
@Temperature 400 °C
174000 psi
@Temperature 752 °F
 1225 MPa
@Temperature 200 °C
177700 psi
@Temperature 392 °F
 1400 MPa
@Temperature 23.0 °C
203000 psi
@Temperature 73.4 °F
Tensile Strength, Yield  100 MPa
@Temperature 750 °C
14500 psi
@Temperature 1380 °F
 650 MPa
@Temperature 600 °C
94300 psi
@Temperature 1110 °F
 900 MPa
@Temperature 400 °C
131000 psi
@Temperature 752 °F
 1100 MPa
@Temperature 200 °C
160000 psi
@Temperature 392 °F
 1300 MPa
@Temperature 23.0 °C
189000 psi
@Temperature 73.4 °F
Modulus of Elasticity 115 GPa16700 ksiTypical
 100 GPa
@Temperature 425 °C
14500 ksi
@Temperature 797 °F
 107 GPa
@Temperature 315 °C
15500 ksi
@Temperature 599 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000190 - 0.000205 ohm-cm0.000190 - 0.000205 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 100 °C
5.00 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.502 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 7.61 W/m-K52.8 BTU-in/hr-ft²-°F
Melting Point 1595 - 1675 °C2903 - 3047 °F
Solidus 1595 °C2903 °F
Liquidus 1675 °C3047 °F
Beta Transus 940 °C1720 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.5 %5.5 - 6.5 %
Carbon, C <= 0.040 %<= 0.040 %
Hydrogen, H <= 0.125 %<= 0.125 %
Iron, Fe <= 0.15 %<= 0.15 %
Molybdenum, Mo 5.5 - 6.5 %5.5 - 6.5 %
Nitrogen, N <= 0.040 %<= 0.040 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.15 %<= 0.15 %
Tin, Sn 1.75 - 2.25 %1.75 - 2.25 %
Titanium, Ti 79.4 - 83.7 %79.4 - 83.7 %Calculated as remainder
Zirconium, Zr 3.6 - 4.4 %3.6 - 4.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 20% Elongated Alpha + STA
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Beta Forged + STA
AISI Type 304L Stainless Steel
AISI Type 304L Stainless Steel, Annealed Bar, Longitudinal
AISI 304L Cast Stainless Steel, UNS J92620

NTIME6246I / 200039

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.