PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injection moulded, extruded, blow moulded and blown into film. Surface resistance values of 109 O (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved. The products made out of PRE-ELEC® ESD 5510 are washable, reusable and recyclable. PRE-ELEC® ESD 5510 is designed for clean applications with extremely low amount of extractable ions. The melt flow properties of PRE-ELEC® ESD 5510 are tailored to fit the requirements of (co)extrusion. Applications: Bins, trays, bottles and bags where permanent ESD protection and high cleanliness are required. These products can be used mainly in electronics packaging, but in many other application areas as well. Processing: PRE-ELEC® ESD 5510 compound can be processed in normal processing conditions as with polypropylene. Test Specimen: 10[mm] wide moulded rod Information from Premix OY |