MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Eraclene® MM 74 High Density Polyethylene - Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.

Eraclene MM 74 is characterized by a good balance between rigidity and impact resistance. The resin is UV stabilized and is recommended for the production of items for outdoor exposure.

Main Applications: Eraclene MM 74 is specifically designed for pails, lids for light-weight containers, agricultural containers, houseware and dust bins.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.953 g/cc0.953 g/ccISO 1183
Melt Flow  4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 12 g/10 min
@Load 5.00 kg,
Temperature 190 °C
12 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868/A
Tensile Strength at Break 19.0 MPa2760 psiISO 527
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break 600 %600 %ISO 527
Flexural Modulus 1.20 GPa174 ksiISO 178
Izod Impact, Notched 1.30 J/cm2.44 ft-lb/inISO 180/A
 
Thermal PropertiesMetricEnglishComments
Melting Point 134 °C273 °FInternal method
Vicat Softening Point 126 °C
@Load 1.00 kg
259 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Versalis Eraclene® MM 74 U High Density Polyethylene - Injection Molding
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Entec Hypel® PEHD.3/.955 HDPE
Amco PRIMATOP HDPE 055952 Injection Molding Polyethylene

PENG112 / 124506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.