MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Scotch-Weld™ DP640 Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properly abraded and cleaned plastics. Good adhesion can also be obtained on etched aluminum as well as primed aluminum, steel glass. For maximum bond durability under moisture conditions, priming of glass and metal substrates is required.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 25000 cP25000 cP
Brookfield Viscosity 10000 - 40000 cP10000 - 40000 cPBase, RVF #6 sp @ 10 rpm
 15000 - 55000 cP15000 - 55000 cPAccelerator, RVF #5 sp @ 10 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70 - 8070 - 80ASTM D2240
Elongation at Break 100 %100 %ASTM D882
Shear Strength 13.8 MPa2000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.60e+12 ohm-cm2.60e+12 ohm-cmASTM D257
Dielectric Constant 5.9
@Frequency 1000 Hz
5.9
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.5 kV/mm470 kV/inASTM D149
Dissipation Factor 0.12
@Frequency 1000 Hz
0.12
@Frequency 1000 Hz
ASTM D150
 
Processing PropertiesMetricEnglishComments
Cure Time 360 - 480 min6.00 - 8.00 hourTime to Handling Strength
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade)
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M Scotch-Weld™ DP-605NS Off-White Adhesive in Duo-Pak Cartridges
3M Scotch-Weld™ DP420 Black Epoxy Adhesive

PMM34659 / 169406

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.