MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance. Good chemical resistance.

Applications: bonding ceramic wear tips to aluminum, brake pads to metal, assembling and repairing machines, aerospace and automotive applications, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Moisture Absorption at Equilibrium 0.80 %0.80 %
Viscosity 5000 cP5000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Tensile Strength, Ultimate 34.5 MPa5000 psi
Elongation at Break 3.0 %3.0 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cm
Dielectric Strength 19.7 kV/mm500 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 62.0 µm/m-°C
@Temperature 20.0 °C
34.4 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.01 W/m-K7.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Shrinkage 1.0 %1.0 %
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 121 °C
0.250 hour
@Temperature 250 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Atom Adhesives AA-BOND F253 Epoxy Adhesive
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive

PCOTR0400 / 29065

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.