MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

M. Holland Company MTEGRITY™ LL800 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low Warpage

Uses: Containers, Household Goods, Lids, Thin-walled Parts

Approvals: FDA 21 CFR 177.1520(c) 3.2a

Processing Method: Injection Molding

Information provided by M. Holland.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³ASTM D792
Melt Flow 55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength, Yield 16.5 MPa2400 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Flexural Modulus 0.469 GPa68.0 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100 °C212 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow R7021-50RNA Polypropylene Random Copolymer Resin
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE
NIZHNEKAMSKNEFTEKHIM PE 4026Z (26460) Linear Low Density Polyethylene
M. Holland Company MTEGRITY™ HD500 HDPE, Copolymer

PMH054 / 52987

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.