MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik ROHAMERE® 6844-O N-(2-Methacryloyloxyethyl)Ethylene Urea 25% Solution In Methylmethacrylate  (discontinued **)
Categories: Fluid

Material Notes: Application: Polymerization and copolymerization in emulsion and solution. Used in the paint and lacquer industries.

Appearance: Clear, yellowish liquid

Odor: Ester-like

CAS: 96261-90-7

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Viscosity 1.0 cP
@Temperature 20.0 °C
1.0 cP
@Temperature 68.0 °F
Vapor Pressure 0.0387 bar
@Temperature 20.0 °C
29.0 torr
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100.3 °C
@Pressure 0.1013 MPa
212.5 °F
@Pressure 14.69 psi
Flash Point 10.0 °C50.0 °FDIN 51755
Ignition Temperature 430 °C806 °FDIN 51794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.433 - 1.443
@Temperature 20.0 °C
1.433 - 1.443
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %Rohm Method: M3 (according to K. Fischer)
 
Descriptive Properties
Colormax. 200Rohm Method: M5 (Pt-Co)
Content N-(2-Methacryloyloxyethyl)ethylene urea (%)23-27Rohm Method: M2-4 (GC)
Explosion limits in air (Vol. %)2.1-12.5
MEHQ400-600ppm, Rohm Method: M1-1 (HPLC), MEHQ
 50-100ppm, Rohm Method: M1-3 (HPLC), Phenothiazine
Methylmethacrylate Content (%)68-78Rohm Method: M2-4 (GC)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials Tantalum Carbide (TaC) Coating
H.C. Starck Baymetec® Tantalum Ethoxide
Evonik ROHAMERE® 6852-O N-(2-Methacryloyloxyethyl)Ethylene Urea 50% Solution In Water
C-Glass Fiber, Generic
Beijing Evergrow Resources UHMW PE Powder

PCYR00112 / 101101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.