MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay ANTAROX® BL 214 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: ETHOXYLATED PROPOXYLATED C8-C10 ALCOHOLS

CAS: 68603-25-8; 7732-18-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ANTAROX© BL-214 functions as a good foam control surfactant with excellent rewetting properties at temperatures as low as 25° C. ANTAROX© BL-214 is soluble in water and polar solvents. ANTAROX© BL-214 is used in ambient temperature spray metal cleaners, polyacrylamide emulsions, and textile finishing operations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 3.0<= 3.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Slightly Hazy, Free Flowing LiquidRP-0064
Cloud point12-16°C1% Solution, RP-0124
Neutralization Number<0.5 mg KOH/mgpH 7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ANTAROX® BL 240 Surfactant
Solvay ANTAROX® BL 225 E Surfactant
Solvay ANTAROX® BL 480 Surfactant
Solvay ANTAROX® L 61 Surfactant
Solvay ANTAROX® BL 330 Surfactant

WRHOD073 / 137304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.