Esenttia 12R88A Random Copolymer Polypropylene
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
Material Notes:
Characteristics: Control reologhy Random copolymer polypropylene; good impact resistance; with antistatic additive.
Recommended for: General purpose injection molding applications.
Information provided by Esenttia by Propilco
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Melt Flow
12.5
g/10 min
@Load 2.16 kg,
Temperature 230 °C
12.5
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238B
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
25.51
MPa
3700
psi
50 mm/min; ASTM D638
Elongation at Yield
13 %
13 %
50 mm/min; ASTM D638
Flexural Modulus, 1% Secant
896.3
MPa
130000
psi
1.3 mm/min; ASTM D790-1A
Izod Impact, Notched
0.5338
J/cm
1.000
ft-lb/in
ASTM D256-A
Gardner Impact
26.55
J
19.58
ft-lb
ASTM D5420A
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Flint Hills P5G2K-096 Random Copolymer Polypropylene
Esenttia 60R45CD Random Copolymer Polypropylene
Esenttia 45R60CD Random Copolymer Polypropylene
Esenttia 35R80 Random Copolymer Polypropylene
Esenttia 30R40CD Random Copolymer Polypropylene
PESEN036 / 184608
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.