MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radiometal 4550 Ni-Fe Soft Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: Combines excellent permeability with high saturation flux density. Used for sensitive relays that must respond to very weak currents. Widely used in transformers, chokes and specialty motors.

Information provided by Smiths Metal Centres.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.25 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 130130Hot Rolled
Tensile Strength 470 MPa68200 psiHot Rolled
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.025 %0.025 %
Iron, Fe 54 %54 %As balance
Manganese, Mn 0.30 %0.30 %
Nickel, Ni 45.50 %45.50 %
Silicon, Si 0.25 %0.25 %
 
Descriptive Properties
Magnetic Flux Density B(T)>0.50 at Magnetizing Field H of 16 A/mAfter heat treatment in hydrogen
 >0.90 at Magnetizing Field H of 40 A/mAfter heat treatment in hydrogen
 >1 at Magnetizing Field H of 1600 A/mAfter heat treatment in hydrogen
 >1.40 at Magnetizing Field H of 800 A/mAfter heat treatment in hydrogen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 2 Soft Magnetic Steel
Aperam Supera 50T Cold Rolled Strip
Ed Fagan EFI Alloy 79 Soft Magnetic Alloy
Aperam Permimphy Cold Rolled Strip
Aperam Mumetal Cold Rolled Strip

NZ97900 / 195023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.