MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott DMZ 20 VIS Bandpass Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Spectral range 400-599 nm, +/- 1.0%

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness <= 600 microns<= 23.6 mil
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °Fcontinuous
 100 °C212 °Fintermittent
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 0.0010 %
@Wavelength 600 - 800 nm
>= 0.0010 %
@Wavelength 600 - 800 nm
 <= 45 %
@Wavelength 400 - 449 nm
<= 45 %
@Wavelength 400 - 449 nm
 <= 50 %
@Wavelength 450 - 599 nm
<= 50 %
@Wavelength 450 - 599 nm
 
Descriptive Properties
Blocking rangeUnlimited
Half width (FWHM)18-22 nm
Q=(tenth width/half width)1.8
q=(thousandth width/half width)6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unipetrol PE HD LITEN® MB/ML 87 HDPE
Unipetrol PE HD LITEN® MB/ML 77 HDPE
Unipetrol PE HD LITEN® LS 87 HDPE
Techmer ES HiFill® HDPE UV
RTP Company RTP 700 UV High Density Polyethylene (HDPE), UV Stabilized

CSGT9807 / 183060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.