MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP Lubricomp® DCL-4036 Polycarbonate, Carbon Fiber Reinforced, PTFE Lubricant  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon + PTFE Filled

Material Notes:
  • Features: Lubricated, Electrically Conductive
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccMethod A; ASTM D792
Linear Mold Shrinkage 0.00 - 0.0010 cm/cm0.00 - 0.0010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 159 MPa23100 psiASTM D638
Elongation at Break 1.7 %1.7 %ASTM D638
Flexural Strength 241 MPa35000 psiASTM D790
Flexural Modulus 17.9 GPa2600 ksiASTM D790
Izod Impact, Notched 1.23 J/cm
@Thickness 3.18 mm
2.30 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.18 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.430.43vs. Steel - @ 40 psi, 50 ft/min, tested in accordance with LNP WI-0687; ASTM D1894
Coefficient of Friction, Static 0.340.34vs. Steel @ 40 psi, in accordance with LNP WI-0687; ASTM D1894
K (wear) Factor 76.5 x 10-8 mm³/N-M38.0 x 10-10 in³-min/ft-lb-hr40psi, 50ft/min; tested in accordance with LNP WI-0687
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm - 1e+0510000 ohm-cm - 1e+05ASTM D257
Surface Resistance 1000 - 10000 ohm1000 - 10000 ohmASTM D4496
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 304 - 327 °C579 - 621 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.172 - 0.345 MPa24.9 - 50.0 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 385 TFE 20  Polycarbonate (PC) Carbon Fiber 30% - PTFE 20%
RTP Company RTP 399 X 113385 B Polycarbonate (PC); LDS Platable
LNP Lubricomp® DL-4030 Polycarbonate, PTFE Additive
ChevronTexaco Mechanism LPS® ISO 15 Hydraulic Oil
ASTM A514 Steel, grade P, plate thickness ≤ 19 mm

PZLNP1126 / 51208

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.