MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Capron® 5202 HS Blend Nylon 66 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as well as excellent chemical resistance. The addition of heat stabilizer system extends the retention of properties at elevated temperatures.

Capron 5202 HS Blend is generally recommended for slightly higher temperature and stiffness requirements, such as engine components, power tool guides, straps and other hardware.

Data provided by Allied Signal.

Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 280-305 degC (536-581 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 45 degC (113 degF) and as high as 105 degC (221 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO data
Moisture Absorption at Equilibrium 2.5 %2.5 %50% RH; 23°C; ISO data
Water Absorption at Saturation 8.5 %8.5 %in water; 23°C; ISO data
Viscosity Measurement 5555Formic Acid Viscosity; ISO data
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM Data MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psiASTM value at 50 mm/min.
 86.0 MPa12500 psiISO value at 50 mm/min.
Elongation at Break 15 %15 %Nominal
 15 %15 %Nominal
Elongation at Yield 5.0 %5.0 %ISO Value at 50 mm/min.
 5.0 %5.0 %ASTM Value at 50 mm/min.
Flexural Yield Strength 130 MPa18900 psiASTM Data
Flexural Modulus 3.14 GPa455 ksiASTM Data
Poissons Ratio 0.350.35ISO data
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FASTM Data
 80.0 °C176 °FISO data
Flammability, UL94  V-2
@Thickness 0.700 mm
V-2
@Thickness 0.0276 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
Akro-Plastic Akromid® C3 1 (4546) PA66/6 Conditioned
Asahi Kasei Leona™ 90G33 Polyamide 66, GF Reinforced
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Conditioned)
MTI ThermoStran® TPU-40G Long Glass Fiber Compound

PALC07 / 23801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.