MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Johnson Matthey Orobraze™ 950 Gold Bearing Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: Orobraze™ 950 is a high purity gold bearing brazing filler metal. It is extensively used in aerospace components and thermionic valve / vacuum tube devices as well as in other specialized applications.

Orobraze™ 950 exhibits excellent high temperature strength up to 500°C and oxidation resistance up to 800°C. Because of the alloy’s elevated temperature properties it is used extensively in the manufacture of components required to operate at high temperature, for example turbojet aero-engine components. The alloy produces small exceptionally smooth fillets at the joint edges that do not disturb the aerodynamic gas flow in aero-engine components.

Orobraze™ 950 is suitable for vacuum furnace brazing, as it contains no volatile elements. Grade 1 Orobraze™ 950 has impurity levels which make it suitable for brazing components that operate at elevated temperatures in ultra high vacuum, such as vacuum tube devices. It is also suitable for step brazing in complex assemblies.

Orobraze™ 950 also offers good corrosion resistance in many chemical environments and its joints are resistant to interfacial crevice corrosion on stainless steels in aqueous service environments. These properties have been put to use in the paper making industries for example. Typical joint gaps are in the range of 0.025-0.1mm depending on parent metals, joint configuration and brazing methods.

Typical applications are for brazing stainless steel, high temperature nickel alloys and super alloys. It can be used for joining copper to these alloys in thermionic valve devices.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 950 °C1740 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au 82 %82 %
Nickel, Ni 18 %18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Orobraze™ 910 Gold-Copper Brazing Filler Metal
Johnson Matthey Orobraze™ 940 Gold-Copper Brazing Filler Metal
Johnson Matthey Orobraze™ 970 Gold-Copper Brazing Filler Metal
Johnson Matthey Orobraze™ 990 Gold Brazing Alloy
Johnson Matthey Orobraze™ 1270 Precious Metal Brazing Filler Metal

NJMMJ9744 / 186145

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.