MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Channel Industries 5500 Lead Zirconate Titanate Piezoelectric  (discontinued **)
Categories: Ceramic; Oxide; Zirconium Oxide; Piezoelectric

Material Notes: Navy Type II

Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used material for electro-mechanical and electro-acoustic transducers.

Uses of this grade include: Hydrophones; Shallow; Vibration Pickups; Accelerometers; Receiver Transducers; High Static Motion Transducers; Non-Destructive Testing; Audible Alarms

Data provided by Channel Industries, Inc.

Channel Industries was acquired by Piezo Kinetics in 2017.

Key Words: PZT; Lead Zirconium Titanium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 7.60 g/cc>= 0.275 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 28.0 MPa4060 psiDynamic tensile strength
 76.0 MPa11000 psiStatic
 
Electrical PropertiesMetricEnglishComments
Curie Temperature >= 350 °C>= 662 °F
Dielectric Constant 17501750Free dielectric constant KT3
 17751775KT1
Dissipation Factor 0.0200.020Low Field
Piezoelectric Longitudinal Coupling Factor, k33 0.730.73
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -185-185
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 625625
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 25.825.8
Piezoelectric Planar Coupling Factor, kp -0.620-0.620
Piezoelectric Mechanical Q 7575
Piezoelectric Shear Coupling Factor, k15 0.710.71
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 400400
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -11.9-11.9
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 4040
Piezoelectric Transverse Coupling Factor, k31 -0.370-0.370

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Channel Industries 5400 Lead Zirconate Titanate Piezoelectric
CeramTec Sonox® P51 Piezoceramic
CeramTec Sonox® P5 Piezoceramic
Channel Industries 300 Barium Titanate Piezoelectric
CeramTec Sonox® P53 Piezoceramic

CCHAN4 / 727

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.