MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 15R10 Strip steel
Categories: Metal; Ferrous Metal; Austenitic

Material Notes: Sandvik 15R10 is an austenitic chromium nickel (CrNi) stainless steel used as a base material for Sandvik coated strip steel. The product is particularly suited to many types of electric load carrying spring applications, such as contact springs and tactile domes. Sandvik 15R10 is characterized by good corrosion resistance, mechanical strength and excellent fatigue and relaxation properties, as well as superior contact properties and/or solderability, achieved through the right choice of coating layer.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 185 GPa26800 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.5 µm/m-°C
@Temperature 20.0 - 100 °C
8.61 µin/in-°F
@Temperature 68.0 - 212 °F
 16.0 µm/m-°C
@Temperature 20.0 - 200 °C
8.89 µin/in-°F
@Temperature 68.0 - 392 °F
 16.5 µm/m-°C
@Temperature 20.0 - 300 °C
9.17 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity  15.0 W/m-K
@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 16.0 W/m-K
@Temperature 100 °C
111 BTU-in/hr-ft²-°F
@Temperature 212 °F
 19.0 W/m-K
@Temperature 300 °C
132 BTU-in/hr-ft²-°F
@Temperature 572 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 - 0.15 %0.050 - 0.15 %
Chromium, Cr 16 - 19 %16 - 19 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.80 %<= 0.80 %
Nickel, Ni 6.0 - 9.5 %6.0 - 9.5 %
Nitrogen, N <= 0.11 %<= 0.11 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.5 %<= 1.5 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin, Sn
Overview of materials for Low Carbon Steel
Kaneka PHBH Semi-Rigid Bio-based Polymer
Kaneka PHBH Rigid Bio-based Polymer

NSANDV5075 / 199639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.