MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis RB707CF Polypropylene Random Copolymer for Blown Film
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: RB707CF is a propylene-ethylene copolymer film resin without slip and antiblock additives, suitable for the manufacturing of unoriented film on blown film process.

RB707CF is especially suitable for Transparent packaging film (e.g. FFS), sealing layer in coextrusions, textile packaging, food packaging, lamination film, label film, and technical and protection film.

Former trade name for this product was Borclear™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.910 g/cc0.0325 - 0.0329 lb/in³ISO 1183
Thickness 40.0 microns1.57 mil
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 700 %700 %ISO 527-3
Film Elongation at Break, TD 800 %800 %ISO 527-3
Flexural Modulus 0.800 GPa116 ksiISO 178
Secant Modulus, MD 0.750 GPa109 ksiISO 527-3
Secant Modulus, TD 0.850 GPa123 ksiISO 527-3
Impact 3434Damaging Force (N); ISO 7765-2
Impact Test 5.00 J3.69 ft-lbPenetration Energy; ISO 7765-2
Coefficient of Friction >= 0.70>= 0.70Film/Film; ISO 8295
Film Tensile Strength at Break, MD 30.0 - 50.0 MPa4350 - 7250 psiISO 527-3
Film Tensile Strength at Break, TD 35.0 - 55.0 MPa5080 - 7980 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 143 - 147 °C289 - 297 °FISO 3146
Vicat Softening Point 125 °C257 °FISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 8.0 %<= 8.0 %ASTM D1003
Gloss >= 70 %>= 70 %At 20°C; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Esenttia 08H85-1 Homopolymer Polypropylene
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
LyondellBasell Hostalen GC 7260 F2 High Density Polyethylene (HDPE), Extruded
Borealis Borclear™ RE936CF Polypropylene Random Copolymer
Borealis BC918CF Polypropylene Copolymer

PBOREA039 / 27346

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.