MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for exterior applications and painted or plated for special decorative effects. Nucrel® 925 has excellent tensile strength and low temperature impact properties.

Typical Applications:

  • Footwear
  • Powder coating
  • Wire and cable
  • Metal coating
  • Injection molding

Features:

  • Good adhesion to metal and polar substrates
  • Good mold flow to reduce molding cycle time
  • Can be cryogenically ground into a powder
  • Low specific gravity-lightweight

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Index of Compound 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050Initial (peak) hardness; ASTM D2240
Tensile Strength at Break 25.0 MPa3630 psiType IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Elongation at Break 520 %520 %Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Flexural Modulus 0.0740 GPa10.7 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Tensile Impact Strength  275 kJ/m²
@Temperature -40.0 °C
131 ft-lb/in²
@Temperature -40.0 °F
ASTM D1822S
 755 kJ/m²
@Temperature 23.0 °C
359 ft-lb/in²
@Temperature 73.4 °F
ASTM D1822S
 
Thermal PropertiesMetricEnglishComments
Melting Point 74.0 - 92.0 °C165 - 198 °FASTM D3418(DSC)
Vicat Softening Point 67.0 °C153 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 182 °C360 °F
Zone 3 193 °C379 °F
Zone 4 204 °C399 °F
Zone 5 204 °C399 °F
Die Temperature 204 °C400 °F
Melt Temperature 149 - 232 °C300 - 450 °F
 
Descriptive Properties
Methacrylic Acid Content15 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Dow Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Dow Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating

PDUPM107 / 33774

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.