MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel Nitriding #135 Modified Steel, AISI 4140 Modified
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel

Material Notes: Nitriding #135 steel is a modification of AISI 4140 specifically designed to be nitrided for high surface hardness and abrasion resistance.

Information provided by Crucible Industries

Key Words: AISI 4140 Modified
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 28 - 3028 - 30
Hardness, Rockwell HR30N 8686at surface
 62
@Thickness 0.508 mm
62
@Thickness 0.0200 in
 70
@Thickness 0.381 mm
70
@Thickness 0.0150 in
 82
@Thickness 0.254 mm
82
@Thickness 0.0100 in
 84
@Thickness 0.203 mm
84
@Thickness 0.00800 in
 86
@Thickness 0.127 mm
86
@Thickness 0.00500 in
 87
@Thickness 0.0762 mm
87
@Thickness 0.00300 in
Hardness, Vickers 11101110at surface
 420
@Thickness 0.508 mm
420
@Thickness 0.0200 in
 600
@Thickness 0.381 mm
600
@Thickness 0.0150 in
 950
@Thickness 0.254 mm
950
@Thickness 0.0100 in
 1040
@Thickness 0.203 mm
1040
@Thickness 0.00800 in
 1120
@Thickness 0.127 mm
1120
@Thickness 0.00500 in
 1140
@Thickness 0.0762 mm
1140
@Thickness 0.00300 in
Modulus of Elasticity 207 GPa30000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.6 µm/m-°C
@Temperature 21.1 - 121 °C
7.00 µin/in-°F
@Temperature 70.0 - 250 °F
 12.8 µm/m-°C
@Temperature 21.1 - 204 °C
7.10 µin/in-°F
@Temperature 70.0 - 400 °F
 13.0 µm/m-°C
@Temperature 21.1 - 427 °C
7.25 µin/in-°F
@Temperature 70.0 - 800 °F
Thermal Conductivity 41.5 W/m-K
@Temperature 93.3 °C
288 BTU-in/hr-ft²-°F
@Temperature 200 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.15 %1.15 %
Carbon, C 0.40 %0.40 %
Chromium, Cr 1.6 %1.6 %
Iron, Fe 95.6 %95.6 %as balance
Manganese, Mn 0.60 %0.60 %
Molybdenum, Mo 0.35 %0.35 %
Silicon, Si 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Crucible Steel MAXEL® Tooling Alloy Steel, AISI 4140 Modified
Latrobe LSS™ 4140 Alloy Steel (AISI 4140)
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
AISI 4140 Steel, oil quenched, 13 mm (0.5 in.) round [845°C (1550°F) quench, 540°C (1000°F) temper]

NCRUC919 / 160370

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.